SAE AMS 5702D:2007 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings,

SAE AMS 5702D:2007 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings, 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti, Consumable Electrode Remelted or Vacuum Induction Melted, 1750 °F (954 °C) Solution Heat Treated. Composition similar to UNS N09706.